研究了DD483合金在服役温度附近经喷砂处理和退火后的组织演变和表面再结晶行为.将DD483合金试样在0.4~0.7 MPa的压力范围内进行喷......
Quantifying the Influences of Carbides and Porosities on the Fatigue Crack Evolution of a Ni-Based S
The detrimental effects of carbides and porosity on the fatigue crack initiation and propagation of nickel-based single-......
Influence of Ta/Al ratio on the microstructure and creep property of a Ru-containing Ni-based single
Two alloys with different Ta and Al contents were applied to study the influence of Ta/Al ratio on the microstructural e......
Hot-corrosion behavior associated with the evolution of corrosion scales of a Ni-based superalloy in
The degradation of Ni-based superalloys in molten salts is closely related with the evolution of corrosion scales. In th......
Three kinds of superalloys were prepared by spray deposited process.The analysis results of microstructures and mechanic......
The microstructural evolution in Re-containing Ni-based single crystal superalloys with different Tan-talum(Ta)content(2......